Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: UltiMaker, Cleveland-Cliffs, Covestro, Steel Construction Institute, BASF
Plastic Nylon
Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
3
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
5
Ultramid (PA) Product RangeBASFPlastic Nylon · Thermal conductivity: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)Plastic Nylon · Thermal expansion: base material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 CPlastic Nylon · Specific heat: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Plastic Nylon stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 63.1 MPa for Plastic Nylon (3.82x).
Which is lighter, Plastic Nylon or Stainless Steel 304?
Plastic Nylon is lighter: 1,140 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, Plastic Nylon or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 2.33 GPa for Plastic Nylon, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, Plastic Nylon or Stainless Steel 304?
For the same stiffness or strength: Plastic Nylon is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic Nylon
Stainless Steel 304
Stiff rod or tie (tension)
11.8x heavier
lighter
Stiff beam (bending)
29% heavier
lighter
Stiff panel or plate
lighter
1.62x heavier
Strong rod or tie
lighter
1.84x heavier
Strong beam
lighter
2.88x heavier
Strong panel or plate
lighter
3.6x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Plastic Nylon or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.33 W/m·K for Plastic Nylon.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 100 µm/m·K for Plastic Nylon.