Materials / Compare

Plastic Nylon vs. Steel AISI 1045

Compare Plastic Nylon vs. Steel AISI 1045 strength, stiffness, weight and thermal properties.

Plastic Nylon3D printed (FDM)
Steel AISI 1045Wrought
MechanicalPlastic NylonSteel AISI 1045
Yield strength63.1MPa1producer-stated531MPa28.42x stronger
Ultimate tensile strength63.1MPa1producer-stated627MPa29.94x stronger
Flexural strength82.9MPa1not sourced
Elongation at breaknot sourcedin 2 in12%2
Young's modulus (stiffness)2.33GPa1210GPa390.1x stiffer
Density1,140kg/m³16.84x lighter7,800kg/m³3
Strength to weight55.4kN·m/kg68.1kN·m/kg23% higher
Stiffness to weight2.04MN·m/kg26.9MN·m/kg13.2x higher
Poisson's ratiobase material0.440.33
Shear modulus0.833GPa80.8GPa97x stiffer in shear
Bulk modulus3.89GPa175GPa45x higher
Speed of sound1,430m/s5,189m/s3.63x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel AISI 1045
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPURubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel AISI 1045
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic NylonSteel AISI 1045
Thermal conductivitybase material0.33W/m·K540–45W/m·K3
Thermal expansionbase material98–102µm/m·K512µm/m·K3
100 mm part over a 50 °C swing500µm growth60µm growth8.33x less
Specific heatbase material1,700J/kg·K5460–480J/kg·K3
Heats up and cools (diffusivity)0.17mm²/s11.6mm²/s68.1x faster
Thermal shock resistance53.6W/m6,269W/m117x more resistant
Melting point188°C1not sourced
Glass transition55.1°C1not sourced
Max service temperatureHDT 0.455 MPa89.2°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel AISI 1045
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic NylonSteel AISI 1045
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: UltiMaker, Niagara LaSalle, Ovako, Covestro, BASF
Plastic Nylon
Ultimaker Nylon, 3D-printed specimens, XY (flat), conditioned >=24 h at room temperature; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v2.00, April 20, 2022.
Steel AISI 1045
AISI 1045 cold drawn bar (Niagara LaSalle) for mechanical; Ovako C45 (lists 'SAE 1045' as a similar designation) for physical constants
  1. 1
    Ultimaker Nylon Technical Data Sheet, v5.00UltiMakerarchived copyPlastic Nylon · Yield strength: typicalPlastic Nylon · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic Nylon · Flexural strength: typicalPlastic Nylon · Young's modulus (stiffness): typicalPlastic Nylon · Density: typicalPlastic Nylon · Melting point: typicalPlastic Nylon · Glass transition: typicalPlastic Nylon · Max service temperature: HDT 0.455 MPa (printed specimens)
  2. 2
    1045 PropertiesNiagara LaSallearchived copySteel AISI 1045 · Yield strength: producer-stated, cold drawnSteel AISI 1045 · Ultimate tensile strength: producer-stated, cold drawnSteel AISI 1045 · Elongation at break: in 2 in (50.8 mm)
  3. 3
    C45 Steel GradeOvakoSteel AISI 1045 · Young's modulus (stiffness): typicalSteel AISI 1045 · Density: typicalSteel AISI 1045 · Poisson's ratio: typicalSteel AISI 1045 · Thermal conductivity: typical range, ambientSteel AISI 1045 · Thermal expansion: typical, mean 20-300 °CSteel AISI 1045 · Specific heat: typical range, 50/100 °C
  4. 4
    Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroPlastic Nylon · Poisson's ratio: base material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)
  5. 5
    Ultramid (PA) Product RangeBASFPlastic Nylon · Thermal conductivity: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)Plastic Nylon · Thermal expansion: base material: unreinforced BASF Ultramid PA66 (A3K, 98) and PA6 (B3S, 102), 23-55 CPlastic Nylon · Specific heat: base material: unreinforced BASF Ultramid PA66 (A3K) and PA6 (B3S), 23 C (same value for both)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic Nylon stronger than Steel AISI 1045?

Steel AISI 1045 is stronger: its yield strength is 531 MPa against 63.1 MPa for Plastic Nylon (8.42x).

Which is lighter, Plastic Nylon or Steel AISI 1045?

Plastic Nylon is lighter: 1,140 kg/m³ against 7,800 kg/m³ for Steel AISI 1045.

Which is stiffer, Plastic Nylon or Steel AISI 1045?

Steel AISI 1045 is stiffer: Young's modulus 210 GPa against 2.33 GPa for Plastic Nylon, so the same part in Steel AISI 1045 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon or Steel AISI 1045?

For the same stiffness or strength: Plastic Nylon is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 1045 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.

Part that must bePlastic NylonSteel AISI 1045
Stiff rod or tie (tension)13.2x heavierlighter
Stiff beam (bending)39% heavierlighter
Stiff panel or platelighter1.53x heavier
Strong rod or tie23% heavierlighter
Strong beamlighter1.65x heavier
Strong panel or platelighter2.36x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Plastic Nylon or Steel AISI 1045?

Steel AISI 1045 conducts heat better: 42.5 W/m·K against 0.33 W/m·K for Plastic Nylon.

Which expands less with temperature?

Steel AISI 1045 expands less: 12 µm/m·K against 100 µm/m·K for Plastic Nylon.

Related comparisons