Plastic PEEK vs. Plastic UHMWPE

Compare Plastic PEEK vs. Plastic UHMWPE strength, stiffness, weight and thermal properties.

Change either side
Plastic PEEKBulk polymer (molded or machined)
Plastic UHMWPEBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength98MPasourcetypical, tensile yield20MPasourcetypical, tensile stress at yield ISO 527, 50 mm/min
Ultimate tensile strengthnot sourced43MPasourcetypical, tensile stress at break ISO 527, 50 mm/min
Compressive strength125MPasourcetypical, 23 Cnot sourced
Flexural strength165MPasourcetypical, flexural stress at yield, 23 Cnot sourced
Elongation at break25%sourcetypical, at break465%sourcetypical, nominal elongation at break ISO 527
Young's modulus (stiffness)4GPasourcetypical (nominal)0.66GPasourcetypical, tensile modulus ISO 527, 1 mm/min
Density1,300kg/m³sourcetypical (crystalline)930kg/m³sourcetypical
Strength to weight75.4kN·m/kg3.51x higher21.5kN·m/kg
Stiffness to weight3.08MN·m/kg4.34x higher0.71MN·m/kg
Poisson's ratio0.38sourcetypicalnot sourced
Shear modulus1.45GPanot sourced
Bulk modulus5.56GPanot sourced
Speed of sound1,754m/s842m/s
Thermal
Thermal conductivity0.29W/m·Ksourcetypical, average, 23 C0.4W/m·Ksourcetypical, unfilled (narrative value, generic Celanese UHMWPE)
Thermal expansion55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)200µm/m·Ksourcetypical, 20 to 100 °C (generic Celanese UHMWPE)
100 mm part over a 50 °C swing275µm growth3.64x less1,000µm growth
Specific heat2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)not sourced
Heats up and cools (diffusivity)0.101mm²/snot sourced
Thermal shock resistance80.1W/mnot sourced
Melting point343°Csourcetypical, DSC130–138°CsourceDSC 10 K/min
Glass transition143°Csourceonset (midpoint 150 C)not sourced
Max service temperature240°CsourceUL 746B RTI, mechanical strength (continuous use index)80°Csourcerecommended max constant operating temperature
Values forVictrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PEEK stronger than Plastic UHMWPE?

Plastic PEEK is stronger: its yield strength is 98 MPa against 20 MPa for Plastic UHMWPE (4.9x).

Which is lighter, Plastic PEEK or Plastic UHMWPE?

Plastic UHMWPE is lighter: 930 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, Plastic PEEK or Plastic UHMWPE?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, Plastic PEEK or Plastic UHMWPE?

For the same stiffness or strength: Plastic PEEK is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PEEKPlastic UHMWPE
Stiff rod or tie (tension)lighter4.34x heavier
Stiff beam (bending)lighter1.76x heavier
Stiff panel or platelighter30% heavier
Strong rod or tielighter3.51x heavier
Strong beamlighter2.06x heavier
Strong panel or platelighter1.58x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PEEK or Plastic UHMWPE?

Plastic UHMWPE conducts heat better: 0.4 W/m·K against 0.29 W/m·K for Plastic PEEK.

Which expands less with temperature?

Plastic PEEK expands less: 55 µm/m·K against 200 µm/m·K for Plastic UHMWPE.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKPlastic UHMWPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKPlastic UHMWPE
Strength against density