Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Victrex, Cleveland-Cliffs, Steel Construction Institute
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
2
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
3
VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
4
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
5
VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Plastic PEEK stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against 98 MPa for Plastic PEEK (2.46x).
Which is lighter, Plastic PEEK or Stainless Steel 304?
Plastic PEEK is lighter: 1,300 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, Plastic PEEK or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 4 GPa for Plastic PEEK, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, Plastic PEEK or Stainless Steel 304?
For the same stiffness or strength: Plastic PEEK is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
Plastic PEEK
Stainless Steel 304
Stiff rod or tie (tension)
7.81x heavier
lighter
Stiff beam (bending)
12% heavier
lighter
Stiff panel or plate
lighter
1.7x heavier
Strong rod or tie
lighter
2.51x heavier
Strong beam
lighter
3.39x heavier
Strong panel or plate
lighter
3.94x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Plastic PEEK or Stainless Steel 304?
Stainless Steel 304 stretches further before it breaks: 55% elongation at break against 25% for Plastic PEEK.
Thermal
Which conducts heat better, Plastic PEEK or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 0.29 W/m·K for Plastic PEEK.
Which expands less with temperature?
Stainless Steel 304 expands less: 16.9 µm/m·K against 55 µm/m·K for Plastic PEEK.