Materials / Compare

Plastic PEEK vs. Stainless Steel 316

Compare Plastic PEEK vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

Plastic PEEKBulk polymer (molded or machined)
Stainless Steel 316Wrought
MechanicalPlastic PEEKStainless Steel 316
Yield strength98MPa1265MPa22.7x stronger
Ultimate tensile strengthnot stated (yield given)583MPa2
Compressive strength125MPa1not sourced
Flexural strength165MPa1not sourced
Elongation at break25%161%22.44x more ductile
Young's modulus (stiffness)4GPa1200GPa250x stiffer
Density1,300kg/m³16.17x lighter8,027kg/m³2
Strength to weight75.4kN·m/kg2.28x higher33kN·m/kg
Stiffness to weight3.08MN·m/kg24.9MN·m/kg8.1x higher
Poisson's ratio0.383design value0.34
Shear modulus1.45GPa76.9GPa53.1x stiffer in shear
Bulk modulus5.56GPa167GPa30x higher
Speed of sound1,754m/s4,992m/s2.85x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKStainless Steel 316
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKStainless Steel 316
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic PEEKStainless Steel 316
Thermal conductivity0.29W/m·K120–100 °C14.6W/m·K250.3x more heat through a fin
Thermal expansion55µm/m·K1mean16.5µm/m·K23.33x less
100 mm part over a 50 °C swing275µm growth82.5µm growth3.33x less
Specific heat2,200J/kg·K54.89x higherat 20 °C450J/kg·K2
Heats up and cools (diffusivity)0.101mm²/s4.04mm²/s39.9x faster
Thermal shock resistance80.1W/m821W/m10.2x more resistant
Melting point343°C1melting range1,390–1,440°C2
Glass transitiononset143°C1not sourced
Max service temperatureUL 746B RTI240°C1oxidation871–899°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKStainless Steel 316
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKStainless Steel 316
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Victrex, ATI, Steel Construction Institute
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
  2. 2
    ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
  3. 3
    VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
  4. 4
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)
  5. 5
    VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Plastic PEEK stronger than Stainless Steel 316?

Stainless Steel 316 is stronger: its yield strength is 265 MPa against 98 MPa for Plastic PEEK (2.7x).

Which is lighter, Plastic PEEK or Stainless Steel 316?

Plastic PEEK is lighter: 1,300 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.

Which is stiffer, Plastic PEEK or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 4 GPa for Plastic PEEK, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Plastic PEEK or Stainless Steel 316?

For the same stiffness or strength: Plastic PEEK is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending).

Part that must bePlastic PEEKStainless Steel 316
Stiff rod or tie (tension)8.1x heavierlighter
Stiff beam (bending)15% heavierlighter
Stiff panel or platelighter1.68x heavier
Strong rod or tielighter2.28x heavier
Strong beamlighter3.18x heavier
Strong panel or platelighter3.75x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PEEK or Stainless Steel 316?

Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 25% for Plastic PEEK.

Thermal

Which conducts heat better, Plastic PEEK or Stainless Steel 316?

Stainless Steel 316 conducts heat better: 14.6 W/m·K against 0.29 W/m·K for Plastic PEEK.

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 55 µm/m·K for Plastic PEEK.

Related comparisons