Mechanical
Yield strength46.2MPasourcetypical20MPasourcetypical, tensile stress at yield ISO 527, 50 mm/min
Ultimate tensile strength46.2MPasourcetypical, peak stress (= stress at yield)43MPasourcetypical, tensile stress at break ISO 527, 50 mm/min
Flexural strength78.9MPasourcetypicalnot sourced
Elongation at break7.6%sourcetypical465%sourcetypical, nominal elongation at break ISO 527
Young's modulus (stiffness)1.94GPasourcetypical0.66GPasourcetypical, tensile modulus ISO 527, 1 mm/min
Density1,270kg/m³sourcetypical930kg/m³sourcetypical37% lighter
Strength to weight36.4kN·m/kg1.69x higher21.5kN·m/kg
Stiffness to weight1.53MN·m/kg2.15x higher0.71MN·m/kg
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,236m/s842m/s
Thermal
Thermal conductivity0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical0.4W/m·Ksourcetypical, unfilled (narrative value, generic Celanese UHMWPE)
Thermal expansion51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical200µm/m·Ksourcetypical, 20 to 100 °C (generic Celanese UHMWPE)
100 mm part over a 50 °C swing255µm growth3.92x less1,000µm growth
Specific heat1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)not sourced
Heats up and cools (diffusivity)0.127mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointnot sourced130–138°CsourceDSC 10 K/min
Glass transition77.4°Csourcetypicalnot sourced
Max service temperature76.2°CsourceHDT 0.455 MPa (printed specimens)80°Csourcerecommended max constant operating temperature
Values forUltimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.Celanese GUR 4120 (avg. molecular weight 4.7x10^6 g/mol), typical values on compression-molded specimens; CTE and thermal conductivity from Celanese's generic UHMWPE guide (grade not named)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PETG stronger than Plastic UHMWPE?

Plastic PETG is stronger: its yield strength is 46.2 MPa against 20 MPa for Plastic UHMWPE (2.31x).

Which is lighter, Plastic PETG or Plastic UHMWPE?

Plastic UHMWPE is lighter: 930 kg/m³ against 1,270 kg/m³ for Plastic PETG.

Which is stiffer, Plastic PETG or Plastic UHMWPE?

Plastic PETG is stiffer: Young's modulus 1.94 GPa against 0.66 GPa for Plastic UHMWPE, so the same part in Plastic PETG deflects less under the same load.

Which is lighter for the same job, Plastic PETG or Plastic UHMWPE?

For the same stiffness or strength: Plastic PETG is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PETGPlastic UHMWPE
Stiff rod or tie (tension)lighter2.15x heavier
Stiff beam (bending)lighter26% heavier
Stiff panel or platelighter5% heavier
Strong rod or tielighter1.69x heavier
Strong beamlighter28% heavier
Strong panel or platelighter11% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PETG or Plastic UHMWPE?

Plastic UHMWPE conducts heat better: 0.4 W/m·K against 0.21 W/m·K for Plastic PETG.

Which expands less with temperature?

Plastic PETG expands less: 51 µm/m·K against 200 µm/m·K for Plastic UHMWPE.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PETGPlastic UHMWPE
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PETGPlastic UHMWPE
Strength against density

Related comparisons