Materials / Compare

Plastic PETG vs. Rubber

Compare Plastic PETG vs. Rubber strength, stiffness, weight and thermal properties.

Change either side
Plastic PETG3D printed (FDM)
RubberBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength46.2MPasourcetypicalnot given (tensile used)
Ultimate tensile strength46.2MPasourcetypical, peak stress (= stress at yield)23MPasourcetypical
Flexural strength78.9MPasourcetypicalnot sourced
Elongation at break7.6%sourcetypical830%sourcetypical109x more ductile
Young's modulus (stiffness)1.94GPasourcetypicalnot sourced
Density1,270kg/m³sourcetypical960kg/m³sourcetypical (specific gravity)
Strength to weight36.4kN·m/kg1.52x higher24kN·m/kg
Stiffness to weight1.53MN·m/kgnot sourced
Poisson's rationot sourced0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound1,236m/snot sourced
Thermal
Thermal conductivity0.21W/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typical0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Thermal expansion51µm/m·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), typicalnot sourced
100 mm part over a 50 °C swing255µm growthnot sourced
Specific heat1,300J/kg·Ksourcebase material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)1,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
Heats up and cools (diffusivity)0.127mm²/s1.52x faster0.0836mm²/s
Thermal shock resistancenot sourcednot sourced
Glass transition77.4°Csourcetypicalnot sourced
Max service temperature76.2°CsourceHDT 0.455 MPa (printed specimens)70°Csourcecontinuous use operating range
Values forUltimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022.Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic PETG stronger than Rubber?

Plastic PETG is stronger: its yield strength is 46.2 MPa against tensile strength 23 MPa for Rubber (2.01x).

Which is lighter, Plastic PETG or Rubber?

Rubber is lighter: 960 kg/m³ against 1,270 kg/m³ for Plastic PETG.

Which is lighter for the same job, Plastic PETG or Rubber?

For the same stiffness or strength: Plastic PETG is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PETGRubber
Strong rod or tielighter1.52x heavier
Strong beamlighter20% heavier
Strong panel or platelighter7% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PETG or Rubber?

Rubber stretches further before it breaks: 830% elongation at break against 7.6% for Plastic PETG.

Which conducts heat better, Plastic PETG or Rubber?

Plastic PETG conducts heat better: 0.21 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PETG
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PETGRubber
Strength against density

Related comparisons