Materials / Compare

Plastic PPS GF40 vs. SLA Resin Standard

Compare Plastic PPS GF40 vs. SLA Resin Standard strength, stiffness, weight and thermal properties.

Plastic PPS GF40Bulk polymer (molded or machined)
SLA Resin Standard3D printed (SLA resin)
MechanicalPlastic PPS GF40SLA Resin Standard
Yield strengthnot given (tensile used)not given (tensile used)
Ultimate tensile strengthtensile strength195MPa13.25x stronger60MPa2
Flexural strength285MPa1105MPa2
Elongation at breakstrain at break1.9%18%24.21x more ductile
Young's modulus (stiffness)14.7GPa15.35x stiffer2.75GPa2
Density1,650kg/m³11,210kg/m³336% lighter
Strength to weight118kN·m/kg2.38x higher49.6kN·m/kg
Stiffness to weight8.91MN·m/kg3.92x higher2.27MN·m/kg
Poisson's ratio0.354not sourced
Shear modulus5.44GPanot sourced
Bulk modulus16.3GPanot sourced
Speed of sound2,985m/s1.98x faster1,508m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PPS GF40SLA Resin Standard
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PPS GF40SLA Resin Standard
Strength against densityHigher and further left: stronger for its weight
ThermalPlastic PPS GF40SLA Resin Standard
Thermal conductivity0.2W/m·K40.54W/m·K52.7x more heat through a fin
Thermal expansionparallel12µm/m·K19.51x lessmean -30 to 140 °C114µm/m·K5
100 mm part over a 50 °C swing60µm growth9.51x less571µm growth
Specific heatnot sourced1,800J/kg·K5
Heats up and cools (diffusivity)not sourced0.248mm²/s
Thermal shock resistance144W/mnot sourced
Melting pointDSC280°C1not sourced
Glass transitionDSC90°C1not sourced
Max service temperatureHDT 1.8 MPa270°C1211 °C hotterHDT 1.8 MPa59°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PPS GF40SLA Resin Standard
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic LCP GF30Plastic PPS GF40SLA Resin Standard
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Celanese, Formlabs
Plastic PPS GF40
Celanese Fortron 1140L4 (PPS, 40% glass fibre), injection moulding; FORTRON PPS Short-Term Properties Guide (PPS-012, 2016); thermal conductivity and Poisson for 40% glass-reinforced Fortron from the Fortron PPS Design Manual (PPS-050, 2013).
SLA Resin Standard
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
  1. 1
    Fortron PPS Short-Term Properties Guide (PPS-012)CelanesePlastic PPS GF40 · Ultimate tensile strength: tensile strength, 5 mm/minPlastic PPS GF40 · Flexural strength: flexural strength at breakPlastic PPS GF40 · Elongation at break: strain at break, 5 mm/minPlastic PPS GF40 · Young's modulus (stiffness): typical, 1 mm/minPlastic PPS GF40 · Density: typicalPlastic PPS GF40 · Thermal expansion: parallel (flow), mean -50 to 90 °CPlastic PPS GF40 · Melting point: DSC, 10 °C/minPlastic PPS GF40 · Glass transition: DSC, 10 °C/minPlastic PPS GF40 · Max service temperature: HDT 1.8 MPa
  2. 2
    Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
  3. 3
    Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
  4. 4
    Fortron PPS Design Manual (PPS-050)CelanesePlastic PPS GF40 · Poisson's ratio: glass-reinforced Fortron PPS (class value, not grade-specific)Plastic PPS GF40 · Thermal conductivity: 40% glass-reinforced Fortron, 25 °C (not grade-specific)
  5. 5
    Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Plastic PPS GF40 stronger than SLA Resin Standard?

Plastic PPS GF40 is stronger: its tensile strength is 195 MPa against 60 MPa for SLA Resin Standard (3.25x).

Which is lighter, Plastic PPS GF40 or SLA Resin Standard?

SLA Resin Standard is lighter: 1,210 kg/m³ against 1,650 kg/m³ for Plastic PPS GF40.

Which is stiffer, Plastic PPS GF40 or SLA Resin Standard?

Plastic PPS GF40 is stiffer: Young's modulus 14.7 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Plastic PPS GF40 deflects less under the same load.

Which is lighter for the same job, Plastic PPS GF40 or SLA Resin Standard?

For the same stiffness or strength: Plastic PPS GF40 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PPS GF40SLA Resin Standard
Stiff rod or tie (tension)lighter3.92x heavier
Stiff beam (bending)lighter1.7x heavier
Stiff panel or platelighter28% heavier
Strong rod or tielighter2.38x heavier
Strong beamlighter1.61x heavier
Strong panel or platelighter32% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Plastic PPS GF40 or SLA Resin Standard?

SLA Resin Standard stretches further before it breaks: 8% elongation at break against 1.9% for Plastic PPS GF40.

Thermal

Which handles higher temperatures, Plastic PPS GF40 or SLA Resin Standard?

Plastic PPS GF40 does: 270 °C against 59 °C for SLA Resin Standard, both HDT 1.8 MPa.

Which conducts heat better, Plastic PPS GF40 or SLA Resin Standard?

SLA Resin Standard conducts heat better: 0.54 W/m·K against 0.2 W/m·K for Plastic PPS GF40.

Which expands less with temperature?

Plastic PPS GF40 expands less: 12 µm/m·K against 114 µm/m·K for SLA Resin Standard.

Related comparisons