Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
EOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.
Stainless Steel 17-4PH
Cleveland-Cliffs 17-4 PH, Condition H 900, sheet/strip, transverse (Product Data Bulletin, May 2021)
1
17-4 PH Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 17-4PH · Yield strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Ultimate tensile strength: typical, transverse, sheet/stripStainless Steel 17-4PH · Elongation at break: typical, transverse, in 2 in. (50.8 mm)Stainless Steel 17-4PH · Young's modulus (stiffness): H 900Stainless Steel 17-4PH · Density: H 900Stainless Steel 17-4PH · Poisson's ratio: H 900 (column)Stainless Steel 17-4PH · Thermal conductivity: at 149 °C (300 °F), H 900Stainless Steel 17-4PH · Thermal expansion: mean, 21–93 °C (70–200 °F), H 900Stainless Steel 17-4PH · Specific heat: mean, 0–100 °C, H 900Stainless Steel 17-4PH · Max service temperature: strength-retention limit (not oxidation)
2
PA 2200 Balance Material Data SheetEOS GmbHSLS PA12 Nylon · Ultimate tensile strength: typicalSLS PA12 Nylon · Elongation at break: typicalSLS PA12 Nylon · Young's modulus (stiffness): typicalSLS PA12 Nylon · Density: typicalSLS PA12 Nylon · Melting point: typicalSLS PA12 Nylon · Max service temperature: HDT 1.8 MPa, X orientation
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLS PA12 Nylon stronger than Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stronger: its yield strength is 1,275 MPa against tensile strength 48 MPa for SLS PA12 Nylon (26.6x).
Which is lighter, SLS PA12 Nylon or Stainless Steel 17-4PH?
SLS PA12 Nylon is lighter: 930 kg/m³ against 7,800 kg/m³ for Stainless Steel 17-4PH.
Which is stiffer, SLS PA12 Nylon or Stainless Steel 17-4PH?
Stainless Steel 17-4PH is stiffer: Young's modulus 197 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Stainless Steel 17-4PH deflects less under the same load.
Which is lighter for the same job, SLS PA12 Nylon or Stainless Steel 17-4PH?
For the same stiffness or strength: SLS PA12 Nylon is lighter for a stiff panel or plate, strong panel or plate; Stainless Steel 17-4PH is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam.
Part that must be
SLS PA12 Nylon
Stainless Steel 17-4PH
Stiff rod or tie (tension)
14.2x heavier
lighter
Stiff beam (bending)
30% heavier
lighter
Stiff panel or plate
lighter
1.7x heavier
Strong rod or tie
3.17x heavier
lighter
Strong beam
6% heavier
lighter
Strong panel or plate
lighter
1.63x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLS PA12 Nylon or Stainless Steel 17-4PH?
SLS PA12 Nylon stretches further before it breaks: 18% elongation at break against 9% for Stainless Steel 17-4PH.