Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Cleveland-Cliffs, EOS GmbH, Steel Construction Institute
SLS PA12 Nylon
EOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
2
PA 2200 Balance Material Data SheetEOS GmbHSLS PA12 Nylon · Ultimate tensile strength: typicalSLS PA12 Nylon · Elongation at break: typicalSLS PA12 Nylon · Young's modulus (stiffness): typicalSLS PA12 Nylon · Density: typicalSLS PA12 Nylon · Melting point: typicalSLS PA12 Nylon · Max service temperature: HDT 1.8 MPa, X orientation
3
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is SLS PA12 Nylon stronger than Stainless Steel 304?
Stainless Steel 304 is stronger: its yield strength is 241 MPa against tensile strength 48 MPa for SLS PA12 Nylon (5.02x).
Which is lighter, SLS PA12 Nylon or Stainless Steel 304?
SLS PA12 Nylon is lighter: 930 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.
Which is stiffer, SLS PA12 Nylon or Stainless Steel 304?
Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Stainless Steel 304 deflects less under the same load.
Which is lighter for the same job, SLS PA12 Nylon or Stainless Steel 304?
For the same stiffness or strength: SLS PA12 Nylon is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending).
Part that must be
SLS PA12 Nylon
Stainless Steel 304
Stiff rod or tie (tension)
13.5x heavier
lighter
Stiff beam (bending)
25% heavier
lighter
Stiff panel or plate
lighter
1.77x heavier
Strong rod or tie
lighter
1.72x heavier
Strong beam
lighter
2.94x heavier
Strong panel or plate
lighter
3.85x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, SLS PA12 Nylon or Stainless Steel 304?
Stainless Steel 304 stretches further before it breaks: 55% elongation at break against 18% for SLS PA12 Nylon.