Materials / Compare

SLS PA12 Nylon vs. Steel AISI 1045

Compare SLS PA12 Nylon vs. Steel AISI 1045 strength, stiffness, weight and thermal properties.

SLS PA12 Nylon3D printed (SLS)
Steel AISI 1045Wrought
MechanicalSLS PA12 NylonSteel AISI 1045
Yield strengthnot given (tensile used)producer-stated531MPa1
Ultimate tensile strength48MPa2producer-stated627MPa113.1x stronger
Elongation at break18%21.5x more ductilein 2 in12%1
Young's modulus (stiffness)1.65GPa2210GPa3127x stiffer
Density930kg/m³28.39x lighter7,800kg/m³3
Strength to weight51.6kN·m/kg68.1kN·m/kg32% higher
Stiffness to weight1.77MN·m/kg26.9MN·m/kg15.2x higher
Poisson's rationot sourced0.33
Shear modulusnot sourced80.8GPa
Bulk modulusnot sourced175GPa
Speed of sound1,332m/s5,189m/s3.9x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000DMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30SLS PA12 NylonSteel AISI 1045
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ADMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30SLS PA12 NylonSteel AISI 1045
Strength against densityHigher and further left: stronger for its weight
ThermalSLS PA12 NylonSteel AISI 1045
Thermal conductivitynot sourced40–45W/m·K3
Thermal expansionnot sourced12µm/m·K3
100 mm part over a 50 °C swingnot sourced60µm growth
Specific heatnot sourced460–480J/kg·K3
Heats up and cools (diffusivity)not sourced11.6mm²/s
Thermal shock resistancenot sourced6,269W/m
Melting point176°C2not sourced
Max service temperatureHDT 1.8 MPa64°C2not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel AISI 1045
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Steel AISI 1045
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Niagara LaSalle, EOS GmbH, Ovako
SLS PA12 Nylon
EOS PA 2200 (PA12) Material Data Sheet, process parameter 'Balance' at 120 µm layer thickness, X orientation, dry (conditioned values not given). Live MDS status 04.10.2026, last changed 10.09.2026; PDF via ?topdf=... link on the same page.
Steel AISI 1045
AISI 1045 cold drawn bar (Niagara LaSalle) for mechanical; Ovako C45 (lists 'SAE 1045' as a similar designation) for physical constants
  1. 1
    1045 PropertiesNiagara LaSallearchived copySteel AISI 1045 · Yield strength: producer-stated, cold drawnSteel AISI 1045 · Ultimate tensile strength: producer-stated, cold drawnSteel AISI 1045 · Elongation at break: in 2 in (50.8 mm)
  2. 2
    PA 2200 Balance Material Data SheetEOS GmbHSLS PA12 Nylon · Ultimate tensile strength: typicalSLS PA12 Nylon · Elongation at break: typicalSLS PA12 Nylon · Young's modulus (stiffness): typicalSLS PA12 Nylon · Density: typicalSLS PA12 Nylon · Melting point: typicalSLS PA12 Nylon · Max service temperature: HDT 1.8 MPa, X orientation
  3. 3
    C45 Steel GradeOvakoSteel AISI 1045 · Young's modulus (stiffness): typicalSteel AISI 1045 · Density: typicalSteel AISI 1045 · Poisson's ratio: typicalSteel AISI 1045 · Thermal conductivity: typical range, ambientSteel AISI 1045 · Thermal expansion: typical, mean 20-300 °CSteel AISI 1045 · Specific heat: typical range, 50/100 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

SLS PA12 Nylon is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is SLS PA12 Nylon stronger than Steel AISI 1045?

Steel AISI 1045 is stronger: its yield strength is 531 MPa against tensile strength 48 MPa for SLS PA12 Nylon (11.1x).

Which is lighter, SLS PA12 Nylon or Steel AISI 1045?

SLS PA12 Nylon is lighter: 930 kg/m³ against 7,800 kg/m³ for Steel AISI 1045.

Which is stiffer, SLS PA12 Nylon or Steel AISI 1045?

Steel AISI 1045 is stiffer: Young's modulus 210 GPa against 1.65 GPa for SLS PA12 Nylon, so the same part in Steel AISI 1045 deflects less under the same load.

Which is lighter for the same job, SLS PA12 Nylon or Steel AISI 1045?

For the same stiffness or strength: SLS PA12 Nylon is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 1045 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.

Part that must beSLS PA12 NylonSteel AISI 1045
Stiff rod or tie (tension)15.2x heavierlighter
Stiff beam (bending)35% heavierlighter
Stiff panel or platelighter1.67x heavier
Strong rod or tie32% heavierlighter
Strong beamlighter1.69x heavier
Strong panel or platelighter2.52x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, SLS PA12 Nylon or Steel AISI 1045?

SLS PA12 Nylon stretches further before it breaks: 18% elongation at break against 12% for Steel AISI 1045.

Related comparisons