Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources4 documents: Kaiser Aluminum, BASF Forward AM, U.S. Department of Defense, INEOS Styrolution
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
FDM HIPS
BASF Forward AM (BASF 3D Printing Solutions) Ultrafuse HiPS, TDS v2.2 (13.11.2019), printed specimens, XY 'Flat'. Specimen print settings are not stated; recommended processing on the sheet: nozzle 240-260 °C, bed 100-120 °C, 40-80 mm/s. Product is discontinued (Forward AM product page) but the TDS is still served by Forward AM.
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM HIPS is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than FDM HIPS?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against tensile strength 18.4 MPa for FDM HIPS (25.5x).
Which is lighter, Aluminum 7050-T7451 or FDM HIPS?
FDM HIPS is lighter: 1,023 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or FDM HIPS?
Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 1.59 GPa for FDM HIPS, so the same part in Aluminum 7050-T7451 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or FDM HIPS?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7050-T7451
FDM HIPS
Stiff rod or tie (tension)
lighter
16x heavier
Stiff beam (bending)
lighter
2.41x heavier
Stiff panel or plate
lighter
28% heavier
Strong rod or tie
lighter
9.21x heavier
Strong beam
lighter
3.13x heavier
Strong panel or plate
lighter
1.83x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7050-T7451 or FDM HIPS?
Aluminum 7050-T7451 stretches further before it breaks: 11% elongation at break against 1.4% for FDM HIPS.
Thermal
Which conducts heat better, Aluminum 7050-T7451 or FDM HIPS?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.17 W/m·K for FDM HIPS.
Which expands less with temperature?
Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 80 µm/m·K for FDM HIPS.