MechanicalAluminum 7050-T7451Plastic HDPE
Yield strength469MPa119.5x stronger24MPa2
Ultimate tensile strength524MPa1not stated (yield given)
Elongation at break11%1not sourced
Young's modulus (stiffness)70.3GPa178.1x stiffer0.9GPa2
Density2,830kg/m³1950kg/m³22.98x lighter
Strength to weight166kN·m/kg6.56x higher25.3kN·m/kg
Stiffness to weight24.8MN·m/kg26.2x higher0.947MN·m/kg
Poisson's ratio0.333base material0.4–0.454
Shear modulus26.4GPa83.7x stiffer in shear0.316GPa
Bulk modulus68.9GPa34.5x higher2GPa
Speed of sound4,984m/s5.12x faster973m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Plastic HDPE
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Plastic HDPE
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 7050-T7451Plastic HDPE
Thermal conductivity157W/m·K1base material0.4–0.49W/m·K4
Thermal expansion23.5µm/m·K15.11x lessbase material120µm/m·K4
100 mm part over a 50 °C swing118µm growth5.11x less600µm growth
Specific heat860J/kg·K1base material2,250J/kg·K42.62x higher
Heats up and cools (diffusivity)64.5mm²/s310x faster0.208mm²/s
Thermal shock resistance29,862W/m525x more resistant56.9W/m
Melting pointmelting range524–635°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Plastic HDPE
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Plastic HDPE
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, LyondellBasell, U.S. Department of Defense, INEOS Olefins & Polymers USA
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
Plastic HDPE
LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values
  1. 1
    Alloy 7050 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7050-T7451 · Yield strength: typical, longitudinal, 0.2% offsetAluminum 7050-T7451 · Ultimate tensile strength: typical, longitudinalAluminum 7050-T7451 · Elongation at break: typical, longitudinalAluminum 7050-T7451 · Young's modulus (stiffness): typicalAluminum 7050-T7451 · Density: nominalAluminum 7050-T7451 · Thermal conductivity: typical, 20 °CAluminum 7050-T7451 · Thermal expansion: typical, mean 20-100 °CAluminum 7050-T7451 · Specific heat: typical, at 100 °CAluminum 7050-T7451 · Melting point: melting range
  2. 2
    Hostalen 23050 B Product DataLyondellBasellPlastic HDPE · Yield strength: typical, tensile stress at yield 23 °C, 50 mm/min ISO 527Plastic HDPE · Young's modulus (stiffness): typical, tensile modulus 23 °C ISO 527Plastic HDPE · Density: typical, ISO 1183
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
  4. 4
    Typical Engineering Properties of High Density PolyethyleneINEOS Olefins & Polymers USAarchived copyPlastic HDPE · Poisson's ratio: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal conductivity: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Thermal expansion: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)Plastic HDPE · Specific heat: base material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 7050-T7451 stronger than Plastic HDPE?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 24 MPa for Plastic HDPE (19.5x).

Which is lighter, Aluminum 7050-T7451 or Plastic HDPE?

Plastic HDPE is lighter: 950 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.

Which is stiffer, Aluminum 7050-T7451 or Plastic HDPE?

Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 0.9 GPa for Plastic HDPE, so the same part in Aluminum 7050-T7451 deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Plastic HDPE?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 7050-T7451Plastic HDPE
Stiff rod or tie (tension)lighter26.2x heavier
Stiff beam (bending)lighter2.97x heavier
Stiff panel or platelighter43% heavier
Strong rod or tielighter6.56x heavier
Strong beamlighter2.44x heavier
Strong panel or platelighter48% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum 7050-T7451 or Plastic HDPE?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.445 W/m·K for Plastic HDPE.

Which expands less with temperature?

Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 120 µm/m·K for Plastic HDPE.