Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than Plastic PMMA?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against tensile strength 80 MPa for Plastic PMMA (5.86x).
Which is lighter, Aluminum 7050-T7451 or Plastic PMMA?
Plastic PMMA is lighter: 1,190 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or Plastic PMMA?
Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 3.3 GPa for Plastic PMMA, so the same part in Aluminum 7050-T7451 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or Plastic PMMA?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7050-T7451
Plastic PMMA
Stiff rod or tie (tension)
lighter
8.96x heavier
Stiff beam (bending)
lighter
1.94x heavier
Stiff panel or plate
lighter
17% heavier
Strong rod or tie
lighter
2.47x heavier
Strong beam
lighter
37% heavier
Strong panel or plate
lighter
2% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7050-T7451 or Plastic PMMA?
Aluminum 7050-T7451 stretches further before it breaks: 11% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Aluminum 7050-T7451 or Plastic PMMA?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 70 µm/m·K for Plastic PMMA.