Materials / Compare

Aluminum 7050-T7451 vs. Rubber

Compare Aluminum 7050-T7451 vs. Rubber strength, stiffness, weight and thermal properties.

Aluminum 7050-T7451Wrought
RubberBulk polymer (molded or machined)
MechanicalAluminum 7050-T7451Rubber
Yield strength469MPa1not given (tensile used)
Ultimate tensile strength524MPa122.8x stronger23MPa2
Elongation at break11%1830%275.5x more ductile
Young's modulus (stiffness)70.3GPa1not sourced
Density2,830kg/m³1960kg/m³22.95x lighter
Strength to weight166kN·m/kg6.92x higher24kN·m/kg
Stiffness to weight24.8MN·m/kgnot sourced
Poisson's ratio0.333government0.54
Shear modulus26.4GPanot sourced
Bulk modulus68.9GPanot sourced
Speed of sound4,984m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Rubber
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 7050-T7451Rubber
Thermal conductivity157W/m·K11,040x more heat through a fin0.151W/m·K5
Thermal expansion23.5µm/m·K1not sourced
100 mm part over a 50 °C swing118µm growthnot sourced
Specific heat860J/kg·K1government1,881J/kg·K42.19x higher
Heats up and cools (diffusivity)64.5mm²/s771x faster0.0836mm²/s
Thermal shock resistance29,862W/mnot sourced
Melting pointmelting range524–635°C1not sourced
Max service temperaturenot sourced70°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Rubber
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Kaiser Aluminum, Weir Minerals, U.S. Department of Defense, National Institute of Standards and Technology, Defense Technical Information Center
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
Rubber
Weir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305
  1. 1
    Alloy 7050 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7050-T7451 · Yield strength: typical, longitudinal, 0.2% offsetAluminum 7050-T7451 · Ultimate tensile strength: typical, longitudinalAluminum 7050-T7451 · Elongation at break: typical, longitudinalAluminum 7050-T7451 · Young's modulus (stiffness): typicalAluminum 7050-T7451 · Density: nominalAluminum 7050-T7451 · Thermal conductivity: typical, 20 °CAluminum 7050-T7451 · Thermal expansion: typical, mean 20-100 °CAluminum 7050-T7451 · Specific heat: typical, at 100 °CAluminum 7050-T7451 · Melting point: melting range
  2. 2
    Linatex Premium Rubber Spec Sheet (WMD0118, 2023)Weir MineralsRubber · Ultimate tensile strength: typicalRubber · Elongation at break: typicalRubber · Density: typical (specific gravity)Rubber · Max service temperature: continuous use operating range
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
  4. 4
    Compressibility of Natural Rubber at Pressures Below 500 kg/cm², J. Res. NBS 68A (1964)National Institute of Standards and Technologyarchived copyRubber · Poisson's ratio: government (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation (0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).)Rubber · Specific heat: government (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
  5. 5
    Thermal Conductivity of Soft Vulcanized Natural Rubber: Selected Values (AD 643325)Defense Technical Information Centerarchived copyRubber · Thermal conductivity: government selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 7050-T7451 stronger than Rubber?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against tensile strength 23 MPa for Rubber (20.4x).

Which is lighter, Aluminum 7050-T7451 or Rubber?

Rubber is lighter: 960 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.

Which is lighter for the same job, Aluminum 7050-T7451 or Rubber?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 7050-T7451Rubber
Strong rod or tielighter6.92x heavier
Strong beamlighter2.53x heavier
Strong panel or platelighter1.53x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 7050-T7451 or Rubber?

Rubber stretches further before it breaks: 830% elongation at break against 11% for Aluminum 7050-T7451.

Thermal

Which conducts heat better, Aluminum 7050-T7451 or Rubber?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.151 W/m·K for Rubber.