Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Kaiser Aluminum, Formlabs, U.S. Department of Defense
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
SLA Resin Standard
Formlabs Clear Resin V5 (FLGPCL05), TDS Rev. 01 March 20, 2024; printed on Form 4 at 100 µm, washed 5 min in >=99% IPA, post-cured 15 min at 60 °C in Form Cure. Orientation not stated.
Clear Resin V5 Technical Data Sheet (2024)Formlabsarchived copySLA Resin Standard · Ultimate tensile strength: typicalSLA Resin Standard · Flexural strength: typicalSLA Resin Standard · Elongation at break: typicalSLA Resin Standard · Young's modulus (stiffness): typicalSLA Resin Standard · Max service temperature: HDT 1.8 MPa
3
Clear Resin V5 Technical Data Sheet (web edition)FormlabsSLA Resin Standard · Density: typical, post-cured (same for 5 min ambient and 15 min at 60 °C), ASTM D792
4
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
5
Thermal Properties of Selected Formlabs SLA ResinsFormlabsSLA Resin Standard · Thermal conductivity: typical, post-cured, ASTM E1530SLA Resin Standard · Thermal expansion: mean -30 to 140 °C, post-cured (5 min ambient cure), TMA ASTM E831SLA Resin Standard · Specific heat: typical, 25 °C, post-cured (5 min ambient cure), DSC ASTM E1269
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Standard is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than SLA Resin Standard?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against tensile strength 60 MPa for SLA Resin Standard (7.82x).
Which is lighter, Aluminum 7050-T7451 or SLA Resin Standard?
SLA Resin Standard is lighter: 1,210 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or SLA Resin Standard?
Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 2.75 GPa for SLA Resin Standard, so the same part in Aluminum 7050-T7451 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or SLA Resin Standard?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Aluminum 7050-T7451
SLA Resin Standard
Stiff rod or tie (tension)
lighter
10.9x heavier
Stiff beam (bending)
lighter
2.16x heavier
Stiff panel or plate
lighter
26% heavier
Strong rod or tie
lighter
3.34x heavier
Strong beam
lighter
1.68x heavier
Strong panel or plate
lighter
20% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7050-T7451 or SLA Resin Standard?
Aluminum 7050-T7451 stretches further before it breaks: 11% elongation at break against 8% for SLA Resin Standard.
Thermal
Which conducts heat better, Aluminum 7050-T7451 or SLA Resin Standard?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.54 W/m·K for SLA Resin Standard.
Which expands less with temperature?
Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 114 µm/m·K for SLA Resin Standard.