Materials / Compare

Aluminum 7050-T7451 vs. Stainless Steel 316

Compare Aluminum 7050-T7451 vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

Aluminum 7050-T7451Wrought
Stainless Steel 316Wrought
MechanicalAluminum 7050-T7451Stainless Steel 316
Yield strength469MPa11.77x stronger265MPa2
Ultimate tensile strength524MPa1583MPa211% stronger
Elongation at break11%161%25.55x more ductile
Young's modulus (stiffness)70.3GPa1200GPa22.84x stiffer
Density2,830kg/m³12.84x lighter8,027kg/m³2
Strength to weight166kN·m/kg5.02x higher33kN·m/kg
Stiffness to weight24.8MN·m/kg24.9MN·m/kg
Poisson's ratio0.333design value0.34
Shear modulus26.4GPa76.9GPa2.91x stiffer in shear
Bulk modulus68.9GPa167GPa2.42x higher
Speed of sound4,984m/s4,992m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Stainless Steel 316
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Stainless Steel 316
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 7050-T7451Stainless Steel 316
Thermal conductivity157W/m·K110.8x more heat through a fin20–100 °C14.6W/m·K2
Thermal expansion23.5µm/m·K1mean16.5µm/m·K242% less
100 mm part over a 50 °C swing118µm growth82.5µm growth42% less
Specific heat860J/kg·K11.91x higherat 20 °C450J/kg·K2
Heats up and cools (diffusivity)64.5mm²/s16x faster4.04mm²/s
Thermal shock resistance29,862W/m36.4x more resistant821W/m
Melting pointmelting range524–635°C1melting range1,390–1,440°C2
Max service temperaturenot sourcedoxidation871–899°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Stainless Steel 316
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Stainless Steel 316
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, ATI, U.S. Department of Defense, Steel Construction Institute
Aluminum 7050-T7451
7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
Stainless Steel 316
ATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
  1. 1
    Alloy 7050 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7050-T7451 · Yield strength: typical, longitudinal, 0.2% offsetAluminum 7050-T7451 · Ultimate tensile strength: typical, longitudinalAluminum 7050-T7451 · Elongation at break: typical, longitudinalAluminum 7050-T7451 · Young's modulus (stiffness): typicalAluminum 7050-T7451 · Density: nominalAluminum 7050-T7451 · Thermal conductivity: typical, 20 °CAluminum 7050-T7451 · Thermal expansion: typical, mean 20-100 °CAluminum 7050-T7451 · Specific heat: typical, at 100 °CAluminum 7050-T7451 · Melting point: melting range
  2. 2
    ATI 316, 316L, 317 and 317L Technical Data Sheet (2012)ATIarchived copyStainless Steel 316 · Yield strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Ultimate tensile strength: typical (representative), annealed 1.0 mm sheetStainless Steel 316 · Elongation at break: typical (representative), annealed, in 2 in. (51 mm)Stainless Steel 316 · Young's modulus (stiffness): typical, in tensionStainless Steel 316 · Density: typicalStainless Steel 316 · Thermal conductivity: 20–100 °CStainless Steel 316 · Thermal expansion: mean, 20–100 °CStainless Steel 316 · Specific heat: at 20 °CStainless Steel 316 · Melting point: melting rangeStainless Steel 316 · Max service temperature: oxidation (scaling) limit in air
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
  4. 4
    Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 316 · Poisson's ratio: design value (structural stainless steels)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 7050-T7451 stronger than Stainless Steel 316?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 265 MPa for Stainless Steel 316 (1.77x).

Which is lighter, Aluminum 7050-T7451 or Stainless Steel 316?

Aluminum 7050-T7451 is lighter: 2,830 kg/m³ against 8,027 kg/m³ for Stainless Steel 316.

Which is stiffer, Aluminum 7050-T7451 or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Stainless Steel 316?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 7050-T7451Stainless Steel 316
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)lighter1.68x heavier
Stiff panel or platelighter2x heavier
Strong rod or tielighter5.02x heavier
Strong beamlighter4.15x heavier
Strong panel or platelighter3.77x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 7050-T7451 or Stainless Steel 316?

Stainless Steel 316 stretches further before it breaks: 61% elongation at break against 11% for Aluminum 7050-T7451.

Thermal

Which conducts heat better, Aluminum 7050-T7451 or Stainless Steel 316?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 14.6 W/m·K for Stainless Steel 316.

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.

Related comparisons