Materials / Compare
DMLS AlSi10Mg Aluminum vs. FDM Polycarbonate
Compare DMLS AlSi10Mg Aluminum vs. FDM Polycarbonate strength, stiffness, weight and thermal properties.
| Mechanical | DMLS AlSi10Mg Aluminum | FDM Polycarbonate |
|---|---|---|
| Yield strength | 270MPa15.07x stronger | 53.3MPa2 |
| Ultimate tensile strength | 450MPa18.44x stronger | 53.3MPa2 |
| Flexural strength | not sourced | 89.4MPa2 |
| Elongation at break | 10.2%1 | 9.2%2 |
| Young's modulus (stiffness) | 72GPa330.1x stiffer | 2.39GPa2 |
| Density | 2,670kg/m³4 | range1,180–1,200kg/m³2 |
| Strength to weight | 101kN·m/kg2.26x higher | 44.8kN·m/kg |
| Stiffness to weight | 27MN·m/kg13.4x higher | 2.01MN·m/kg |
| Poisson's ratio | base material0.335 | base material0.386 |
| Shear modulus | 27.1GPa31.2x stiffer in shear | 0.867GPa |
| Bulk modulus | 70.6GPa21.2x higher | 3.33GPa |
| Speed of sound | 5,193m/s3.66x faster | 1,418m/s |
| Thermal | DMLS AlSi10Mg Aluminum | FDM Polycarbonate |
|---|---|---|
| Thermal conductivity | 110W/m·K1550x more heat through a fin | base material0.2W/m·K7 |
| Thermal expansion | mean 25-100 °C20µm/m·K13.25x less | base material65µm/m·K7 |
| 100 mm part over a 50 °C swing | 100µm growth3.25x less | 325µm growth |
| Specific heat | base material963J/kg·K5 | not sourced |
| Heats up and cools (diffusivity) | 42.8mm²/s | not sourced |
| Thermal shock resistance | 13,819W/m325x more resistant | 42.5W/m |
| Glass transition | not sourced | 108°C2 |
| Max service temperature | not sourced | HDT 0.455 MPa105°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources7 documents: EOS GmbH, UltiMaker, Renishaw, U.S. Department of Defense, Covestro
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- FDM Polycarbonate
- Ultimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 5MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
- 6Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
- 7Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum and FDM Polycarbonate are 3D printed: their properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than FDM Polycarbonate?
DMLS AlSi10Mg Aluminum is stronger: its yield strength is 270 MPa against 53.3 MPa for FDM Polycarbonate (5.07x).
Which is lighter, DMLS AlSi10Mg Aluminum or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 2,670 kg/m³ for DMLS AlSi10Mg Aluminum.
Which is stiffer, DMLS AlSi10Mg Aluminum or FDM Polycarbonate?
DMLS AlSi10Mg Aluminum is stiffer: Young's modulus 72 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in DMLS AlSi10Mg Aluminum deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or FDM Polycarbonate?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam.
| Part that must be | DMLS AlSi10Mg Aluminum | FDM Polycarbonate |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 13.4x heavier |
| Stiff beam (bending) | lighter | 2.44x heavier |
| Stiff panel or plate | lighter | 39% heavier |
| Strong rod or tie | lighter | 2.26x heavier |
| Strong beam | lighter | 31% heavier |
| Strong panel or plate | about equal | about equal |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or FDM Polycarbonate?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
DMLS AlSi10Mg Aluminum expands less: 20 µm/m·K against 65 µm/m·K for FDM Polycarbonate.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- FDM Polycarbonate vs. Plastic Nylon
- FDM Polycarbonate vs. SLA Resin Standard
- FDM Polycarbonate vs. Plastic Polycarbonate
- FDM Polycarbonate vs. Plastic ABS (bulk/injection)