Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
Plastic PMMA
Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)
1
INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
2
PLEXIGLAS GS and XT Technical Information (Ref. No. 211-1)Röhmarchived copyPlastic PMMA · Ultimate tensile strength: typical, 23 °CPlastic PMMA · Compressive strength: compressive yield stress, typicalPlastic PMMA · Flexural strength: typicalPlastic PMMA · Elongation at break: typicalPlastic PMMA · Young's modulus (stiffness): typical, short-termPlastic PMMA · Density: typicalPlastic PMMA · Poisson's ratio: typicalPlastic PMMA · Thermal conductivity: typicalPlastic PMMA · Thermal expansion: 0-50 °CPlastic PMMA · Specific heat: typicalPlastic PMMA · Max service temperature: max. permanent service temperature
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Nickel Inconel 718 stronger than Plastic PMMA?
Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against tensile strength 80 MPa for Plastic PMMA (15.1x).
Which is lighter, Nickel Inconel 718 or Plastic PMMA?
Plastic PMMA is lighter: 1,190 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Plastic PMMA?
Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 3.3 GPa for Plastic PMMA, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Plastic PMMA?
For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie; Plastic PMMA is lighter for a stiff panel or plate, strong beam, strong panel or plate.
Part that must be
Nickel Inconel 718
Plastic PMMA
Stiff rod or tie (tension)
lighter
8.77x heavier
Stiff beam (bending)
lighter
13% heavier
Stiff panel or plate
1.76x heavier
lighter
Strong rod or tie
lighter
2.18x heavier
Strong beam
13% heavier
lighter
Strong panel or plate
1.78x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Nickel Inconel 718 or Plastic PMMA?
Nickel Inconel 718 stretches further before it breaks: 20% elongation at break against 5.5% for Plastic PMMA.
Thermal
Which conducts heat better, Nickel Inconel 718 or Plastic PMMA?
Nickel Inconel 718 conducts heat better: 11.4 W/m·K against 0.19 W/m·K for Plastic PMMA.
Which expands less with temperature?
Nickel Inconel 718 expands less: 13.2 µm/m·K against 70 µm/m·K for Plastic PMMA.