Materials / Compare
Nickel Inconel 718 vs. Plastic POM/Acetal Compare Nickel Inconel 718 vs. Plastic POM/Acetal strength, stiffness, weight and thermal properties.
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Nickel Inconel 718 Wrought Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Plastic POM/Acetal Bulk polymer (molded or machined) Mechanical Nickel Inconel 718 Plastic POM/Acetal Yield strength 1,207 MPa 17.5x stronger 69 MPa Ultimate tensile strength 1,389 MPa 20.1x stronger 69 MPa Compressive strength not sourced 124 MPa Flexural strength not sourced 99 MPa Elongation at break 20 % 75 % 3.75x more ductile Young's modulus (stiffness) 200 GPa 71.4x stiffer 2.8 GPa Density 8,221 kg/m³ 1,420 kg/m³ 5.79x lighter Strength to weight 147 kN·m/kg 3.02x higher 48.6 kN·m/kg Stiffness to weight 24.3 MN·m/kg 12.3x higher 1.97 MN·m/kg Poisson's ratio 0.294 0.35 Shear modulus 77.3 GPa 74.5x stiffer in shear 1.04 GPa Bulk modulus 162 GPa 52x higher 3.11 GPa Speed of sound 4,932 m/s 3.51x faster 1,404 m/s
1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic POM/Acetal Stiffness against densityHigher and further left: stiffer for its weight 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic POM/Acetal Strength against densityHigher and further left: stronger for its weight
Thermal Nickel Inconel 718 Plastic POM/Acetal Thermal conductivity 11.4 W/m·K 28.5x more heat through a fin 0.4 W/m·K Thermal expansion 13.2 µm/m·K 9.24x less mean 122 µm/m·K 100 mm part over a 50 °C swing 66 µm growth 9.24x less 610 µm growth Specific heat 435 J/kg·K average -18 to 100 °C 1,465 J/kg·K 3.37x higher Heats up and cools (diffusivity) 3.19 mm²/s 16.6x faster 0.192 mm²/s Thermal shock resistance 3,680 W/m 70.1x more resistant 52.5 W/m Melting point melting range 1,260–1,336 °C 175 °C Max service temperature 704 °C HDT 1.8 MPa 125 °C
1k 10k 0.1 1 10 100 Density (kg/m³) Thermal conductivity (W/m·K) Plastic PLA Plastic PETG Plastic ABS Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic POM/Acetal Thermal conductivity against densityHigher and further left: spreads more heat for its weight 0.1 1 10 100 10 100 Thermal conductivity (W/m·K) Thermal expansion (µm/m·K) Plastic PETG Plastic ABS Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic POM/Acetal Thermal expansion against thermal conductivityLower and further right: warps less when heated
Sources 3 documents: Special Metals, DuPont
Nickel Inconel 718 INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
Plastic POM/Acetal DuPont Delrin 100 acetal homopolymer, Table 2 'Typical Properties of Delrin Acetal Resins' (ASTM methods), Delrin Design Guide Module III hosted on delrin.com 1 INCONEL alloy 718 (SMC-045) Special Metals archived copy Nickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer2 Delrin Acetal Resin Design Guide, Module III DuPont archived copy Plastic POM/Acetal · Yield strength: typical (single ASTM D638 tensile strength)Plastic POM/Acetal · Ultimate tensile strength: typicalPlastic POM/Acetal · Compressive strength: compressive stress at 10% deformationPlastic POM/Acetal · Flexural strength: flexural yield strength, typicalPlastic POM/Acetal · Elongation at break: typicalPlastic POM/Acetal · Young's modulus (stiffness): typicalPlastic POM/Acetal · Poisson's ratio: typicalPlastic POM/Acetal · Thermal conductivity: typicalPlastic POM/Acetal · Thermal expansion: mean, 29 to 60 °CPlastic POM/Acetal · Specific heat: average -18 to 100 °C, Delrin acetal resins (not grade-specific)Plastic POM/Acetal · Melting point: crystalline melting pointPlastic POM/Acetal · Max service temperature: HDT 1.8 MPa (annealed)3 Delrin 100 Product Data Sheet DuPont Plastic POM/Acetal · Density: typical (DuPont product information for Delrin 100 NC010; 'The data listed here fall within the normal range of product properties')
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Mechanical Is Nickel Inconel 718 stronger than Plastic POM/Acetal? Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 69 MPa for Plastic POM/Acetal (17.5x).
Which is lighter, Nickel Inconel 718 or Plastic POM/Acetal? Plastic POM/Acetal is lighter: 1,420 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Plastic POM/Acetal? Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 2.8 GPa for Plastic POM/Acetal, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Plastic POM/Acetal? For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam; Plastic POM/Acetal is lighter for a stiff panel or plate, strong panel or plate.
Part that must be Nickel Inconel 718 Plastic POM/Acetal Stiff rod or tie (tension) lighter 12.3x heavier Stiff beam (bending) lighter 46% heavier Stiff panel or plate 40% heavier lighter Strong rod or tie lighter 3.02x heavier Strong beam lighter 16% heavier Strong panel or plate 38% heavier lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Nickel Inconel 718 or Plastic POM/Acetal? Plastic POM/Acetal stretches further before it breaks: 75% elongation at break against 20% for Nickel Inconel 718.
Thermal Which conducts heat better, Nickel Inconel 718 or Plastic POM/Acetal? Nickel Inconel 718 conducts heat better: 11.4 W/m·K against 0.4 W/m·K for Plastic POM/Acetal.
Which expands less with temperature? Nickel Inconel 718 expands less: 13.2 µm/m·K against 122 µm/m·K for Plastic POM/Acetal.