Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Special Metals, Cleveland-Cliffs, Steel Construction Institute
Nickel Inconel 718
INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
Stainless Steel 304
Type 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual
1
INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
2
304/304L Stainless Steel Product Data Bulletin (2021)Cleveland-CliffsStainless Steel 304 · Yield strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Ultimate tensile strength: typical, annealed, 70 °F (21 °C)Stainless Steel 304 · Elongation at break: typical, annealed, in 2 in. (50.8 mm)Stainless Steel 304 · Young's modulus (stiffness): typical, in tensionStainless Steel 304 · Density: typicalStainless Steel 304 · Thermal conductivity: at 100 °CStainless Steel 304 · Thermal expansion: mean, 0–100 °CStainless Steel 304 · Specific heat: mean, 0–100 °CStainless Steel 304 · Melting point: melting rangeStainless Steel 304 · Max service temperature: continuous, oxidation (scaling) limit in air
3
Design Manual for Structural Stainless Steel, 4th Edition (P413)Steel Construction Institutearchived copyStainless Steel 304 · Poisson's ratio: design value (structural stainless steels)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Nickel Inconel 718 stronger than Stainless Steel 304?
Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 241 MPa for Stainless Steel 304 (5.01x).
Which is lighter, Nickel Inconel 718 or Stainless Steel 304?
Stainless Steel 304 is lighter: 8,030 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Stainless Steel 304?
Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 193 GPa for Stainless Steel 304, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Stainless Steel 304?
For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff panel or plate.
Part that must be
Nickel Inconel 718
Stainless Steel 304
Stiff rod or tie (tension)
lighter
1% heavier
Stiff beam (bending)
about equal
about equal
Stiff panel or plate
1% heavier
lighter
Strong rod or tie
lighter
4.89x heavier
Strong beam
lighter
2.86x heavier
Strong panel or plate
lighter
2.19x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Nickel Inconel 718 or Stainless Steel 304?
Stainless Steel 304 stretches further before it breaks: 55% elongation at break against 20% for Nickel Inconel 718.
Thermal
Which handles higher temperatures, Nickel Inconel 718 or Stainless Steel 304?
Stainless Steel 304 does: 899 °C against 704 °C for Nickel Inconel 718.
Which conducts heat better, Nickel Inconel 718 or Stainless Steel 304?
Stainless Steel 304 conducts heat better: 16.2 W/m·K against 11.4 W/m·K for Nickel Inconel 718.
Which expands less with temperature?
Nickel Inconel 718 expands less: 13.2 µm/m·K against 16.9 µm/m·K for Stainless Steel 304.