Materials / Plastic
Plastic HDPE
Plastic HDPE strength, stiffness, density and thermal properties, with their source.
A bracket in Plastic HDPE, smooth finish.
| Process | Bulk polymer (molded or machined) |
|---|---|
| Mechanical | |
| Yield strength | 24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 527 |
| Ultimate tensile strength | not sourced |
| Elongation at break | not sourced |
| Young's modulus (stiffness) | 0.9GPasourcetypical, tensile modulus 23 °C ISO 527 |
| Density | 950kg/m³sourcetypical, ISO 1183 |
| Strength to weight | 25.3kN·m/kg |
| Stiffness to weight | 0.947MN·m/kg |
| Poisson's ratio | 0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE) |
| Shear modulus | 0.316GPa |
| Bulk modulus | 2GPa |
| Speed of sound | 973m/s |
| Thermal | |
| Thermal conductivity | 0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE) |
| Thermal expansion | 120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE) |
| 100 mm part over a 50 °C swing | 600µm growth |
| Specific heat | 2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE) |
| Heats up and cools (diffusivity) | 0.208mm²/s |
| Thermal shock resistance | 56.9W/m |
| Values for | LyondellBasell Hostalen 23050 B high density polyethylene, typical ISO values |
Among 59 materials
Compare Plastic HDPE with
Other Plastic
- Plastic HDPE vs. Plastic PLA
- Plastic HDPE vs. Plastic PETG
- Plastic HDPE vs. Plastic ABS
- Plastic HDPE vs. Plastic TPU
- Plastic HDPE vs. Plastic Nylon
- Plastic HDPE vs. Plastic ABS (bulk/injection)
- Plastic HDPE vs. Plastic Polycarbonate
- Plastic HDPE vs. Plastic POM/Acetal
- Plastic HDPE vs. Plastic Nylon PA6
- Plastic HDPE vs. Plastic Nylon PA66
- Plastic HDPE vs. Plastic PEEK
- Plastic HDPE vs. Plastic PTFE
- Plastic HDPE vs. Plastic UHMWPE
- Plastic HDPE vs. Plastic Polypropylene
- Plastic HDPE vs. Plastic PMMA