Materials / Compare
Aluminum 7050-T7451 vs. FDM Polycarbonate
Compare Aluminum 7050-T7451 vs. FDM Polycarbonate strength, stiffness, weight and thermal properties.
| Mechanical | Aluminum 7050-T7451 | FDM Polycarbonate |
|---|---|---|
| Yield strength | 469MPa18.8x stronger | 53.3MPa2 |
| Ultimate tensile strength | 524MPa19.83x stronger | 53.3MPa2 |
| Flexural strength | not sourced | 89.4MPa2 |
| Elongation at break | 11%120% more ductile | 9.2%2 |
| Young's modulus (stiffness) | 70.3GPa129.4x stiffer | 2.39GPa2 |
| Density | 2,830kg/m³1 | range1,180–1,200kg/m³2 |
| Strength to weight | 166kN·m/kg3.7x higher | 44.8kN·m/kg |
| Stiffness to weight | 24.8MN·m/kg12.3x higher | 2.01MN·m/kg |
| Poisson's ratio | 0.333 | base material0.384 |
| Shear modulus | 26.4GPa30.5x stiffer in shear | 0.867GPa |
| Bulk modulus | 68.9GPa20.7x higher | 3.33GPa |
| Speed of sound | 4,984m/s3.51x faster | 1,418m/s |
| Thermal | Aluminum 7050-T7451 | FDM Polycarbonate |
|---|---|---|
| Thermal conductivity | 157W/m·K1785x more heat through a fin | base material0.2W/m·K5 |
| Thermal expansion | 23.5µm/m·K12.77x less | base material65µm/m·K5 |
| 100 mm part over a 50 °C swing | 118µm growth2.77x less | 325µm growth |
| Specific heat | 860J/kg·K1 | not sourced |
| Heats up and cools (diffusivity) | 64.5mm²/s | not sourced |
| Thermal shock resistance | 29,862W/m703x more resistant | 42.5W/m |
| Melting point | melting range524–635°C1 | not sourced |
| Glass transition | not sourced | 108°C2 |
| Max service temperature | not sourced | HDT 0.455 MPa105°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: Kaiser Aluminum, UltiMaker, U.S. Department of Defense, Covestro
- Aluminum 7050-T7451
- 7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J
- FDM Polycarbonate
- Ultimaker PC, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 20, 2022.
- 1Alloy 7050 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7050-T7451 · Yield strength: typical, longitudinal, 0.2% offsetAluminum 7050-T7451 · Ultimate tensile strength: typical, longitudinalAluminum 7050-T7451 · Elongation at break: typical, longitudinalAluminum 7050-T7451 · Young's modulus (stiffness): typicalAluminum 7050-T7451 · Density: nominalAluminum 7050-T7451 · Thermal conductivity: typical, 20 °CAluminum 7050-T7451 · Thermal expansion: typical, mean 20-100 °CAluminum 7050-T7451 · Specific heat: typical, at 100 °CAluminum 7050-T7451 · Melting point: melting range
- 2Ultimaker PC Technical Data Sheet, v5.00UltiMakerarchived copyFDM Polycarbonate · Yield strength: typicalFDM Polycarbonate · Ultimate tensile strength: typical, peak stress (= stress at yield)FDM Polycarbonate · Flexural strength: typicalFDM Polycarbonate · Elongation at break: typicalFDM Polycarbonate · Young's modulus (stiffness): typicalFDM Polycarbonate · Density: rangeFDM Polycarbonate · Glass transition: typicalFDM Polycarbonate · Max service temperature: HDT 0.455 MPa (printed specimens)
- 3MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7050-T7451 · Poisson's ratio: typical (handbook physical constant)
- 4Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyFDM Polycarbonate · Poisson's ratio: base material: polycarbonate family typical (Covestro Part and Mold Design guide, Table 3-1)
- 5Makrolon 2405 Technical Data SheetCovestroFDM Polycarbonate · Thermal conductivity: base material: Covestro Makrolon 2405 injection-molding PC, typical, through-plane, 23 °CFDM Polycarbonate · Thermal expansion: base material: Covestro Makrolon 2405 injection-molding PC, typical, 23-55 °C, parallel
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM Polycarbonate is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Aluminum 7050-T7451 stronger than FDM Polycarbonate?
Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 53.3 MPa for FDM Polycarbonate (8.8x).
Which is lighter, Aluminum 7050-T7451 or FDM Polycarbonate?
FDM Polycarbonate is lighter: 1,190 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.
Which is stiffer, Aluminum 7050-T7451 or FDM Polycarbonate?
Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 2.39 GPa for FDM Polycarbonate, so the same part in Aluminum 7050-T7451 deflects less under the same load.
Which is lighter for the same job, Aluminum 7050-T7451 or FDM Polycarbonate?
For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
| Part that must be | Aluminum 7050-T7451 | FDM Polycarbonate |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 12.3x heavier |
| Stiff beam (bending) | lighter | 2.28x heavier |
| Stiff panel or plate | lighter | 30% heavier |
| Strong rod or tie | lighter | 3.7x heavier |
| Strong beam | lighter | 1.79x heavier |
| Strong panel or plate | lighter | 25% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Aluminum 7050-T7451 or FDM Polycarbonate?
Aluminum 7050-T7451 stretches further before it breaks: 11% elongation at break against 9.2% for FDM Polycarbonate.
Thermal
Which conducts heat better, Aluminum 7050-T7451 or FDM Polycarbonate?
Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 0.2 W/m·K for FDM Polycarbonate.
Which expands less with temperature?
Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 65 µm/m·K for FDM Polycarbonate.
Related comparisons
- Aluminum 7050-T7451 vs. Aluminum 7075-T6
- Aluminum 7050-T7451 vs. Aluminum 2024-T351
- Aluminum 7050-T7451 vs. Aluminum
- Aluminum 7050-T7451 vs. Aluminum 6061-T6
- FDM Polycarbonate vs. Plastic Nylon
- FDM Polycarbonate vs. SLA Resin Standard
- FDM Polycarbonate vs. Plastic Polycarbonate
- FDM Polycarbonate vs. Plastic ABS (bulk/injection)