Materials / Compare

Aluminum 7050-T7451 vs. PCB Board FR-4, 2 copper planes

Compare Aluminum 7050-T7451 vs. PCB Board FR-4, 2 copper planes strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7050-T7451Wrought
PCB Board FR-4, 2 copper planesComposite
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength469MPasourcetypical, longitudinal, 0.2% offsetnot given (tensile used)
Ultimate tensile strength524MPasourcetypical, longitudinal246–385MPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D3039)
Elongation at break11%sourcetypical, longitudinalnot sourced
Young's modulus (stiffness)70.3GPasourcetypical21.9–25.8GPasourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction (ASTM D790-15e2); the copper planes are left out
Density2,830kg/m³sourcenominalnot sourced
Strength to weight166kN·m/kgnot sourced
Stiffness to weight24.8MN·m/kgnot sourced
Poisson's ratio0.33sourcetypical (handbook physical constant)0.171–0.177sourcethe bare laminate's (fr4-370hr), in-plane: cross direction .. length direction
Shear modulus26.4GPa2.6x stiffer in shear10.2GPa
Bulk modulus68.9GPa12.2GPa
Speed of sound4,984m/snot sourced
Thermal
Thermal conductivity157W/m·Ksourcetypical, 20 °Cnot sourced
Thermal expansion23.5µm/m·Ksourcetypical, mean 20-100 °C13–14µm/m·Ksourcethe bare laminate's (fr4-370hr), in-plane X/Y-axis, below Tg (IPC-TM-650 2.4.24C)
100 mm part over a 50 °C swing118µm growth67.5µm growth1.74x less
Specific heat860J/kg·Ksourcetypical, at 100 °Cnot sourced
Heats up and cools (diffusivity)64.5mm²/snot sourced
Thermal shock resistance29,862W/mnot sourced
Melting point524–635°Csourcemelting rangenot sourced
Values for7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5JA whole circuit board read as one orthotropic plate: the JEDEC high-K thermal test board (JESD51-7, "2s2p"), 0.062 in (1.575 mm) thick with two internal solid copper planes 0.0014 in (1 oz) thick, as Texas Instruments SZZA017A Table 1 gives it. Copper C110 and the Isola 370HR laminate from this library; the layers conduct in parallel along the board and in series through it (boardStackup.ts). Its two 0.0028 in trace layers cover little of the board and are left out; vias are ignored. Mechanical values are the bare laminate's.

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 7050-T7451 stronger than PCB Board FR-4, 2 copper planes?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against tensile strength 315 MPa for PCB Board FR-4, 2 copper planes (49%).

Which is stiffer, Aluminum 7050-T7451 or PCB Board FR-4, 2 copper planes?

Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 23.9 GPa for PCB Board FR-4, 2 copper planes, so the same part in Aluminum 7050-T7451 deflects less under the same load.

Which expands less with temperature?

PCB Board FR-4, 2 copper planes expands less: 13.5 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.

Among 73 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451
Strength against density

Related comparisons