Materials / Compare
DMLS AlSi10Mg Aluminum vs. Nickel Inconel 718
Compare DMLS AlSi10Mg Aluminum vs. Nickel Inconel 718 strength, stiffness, weight and thermal properties.
| Mechanical | DMLS AlSi10Mg Aluminum | Nickel Inconel 718 |
|---|---|---|
| Yield strength | 270MPa1 | 1,207MPa24.47x stronger |
| Ultimate tensile strength | 450MPa1 | 1,389MPa23.09x stronger |
| Elongation at break | 10.2%1 | 20%21.96x more ductile |
| Young's modulus (stiffness) | 72GPa3 | 200GPa22.78x stiffer |
| Density | 2,670kg/m³43.08x lighter | 8,221kg/m³2 |
| Strength to weight | 101kN·m/kg | 147kN·m/kg45% higher |
| Stiffness to weight | 27MN·m/kg11% higher | 24.3MN·m/kg |
| Poisson's ratio | base material0.335 | 0.2942 |
| Shear modulus | 27.1GPa | 77.3GPa2.86x stiffer in shear |
| Bulk modulus | 70.6GPa | 162GPa2.29x higher |
| Speed of sound | 5,193m/s5% faster | 4,932m/s |
| Thermal | DMLS AlSi10Mg Aluminum | Nickel Inconel 718 |
|---|---|---|
| Thermal conductivity | 110W/m·K19.65x more heat through a fin | 11.4W/m·K2 |
| Thermal expansion | mean 25-100 °C20µm/m·K1 | 13.2µm/m·K21.52x less |
| 100 mm part over a 50 °C swing | 100µm growth | 66µm growth1.52x less |
| Specific heat | base material963J/kg·K5 | 435J/kg·K2 |
| Heats up and cools (diffusivity) | 42.8mm²/s13.4x faster | 3.19mm²/s |
| Thermal shock resistance | 13,819W/m3.76x more resistant | 3,680W/m |
| Melting point | not sourced | melting range1,260–1,336°C2 |
| Max service temperature | not sourced | 704°C2 |
| Try it on a partA bracket to run stress or thermal on, free in your browser | Open in LessCAD | Open in LessCAD |
|---|
Sources5 documents: EOS GmbH, Special Metals, Renishaw, U.S. Department of Defense
- DMLS AlSi10Mg Aluminum
- EOS Aluminium AlSi10Mg (powder 9011-0024), EOS M 290 | 30 µm process (AlSi10Mg_FlexM291 2.01), as manufactured, horizontal; machined (turned) specimens, ISO 6892-1 B10
- Nickel Inconel 718
- INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
- 1EOS Aluminium AlSi10Mg Material Data SheetEOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Yield strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Ultimate tensile strength: typical, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Elongation at break: typical at break, as manufactured, horizontalDMLS AlSi10Mg Aluminum · Thermal conductivity: typical, as manufactured, horizontal (ISO 22007-2)DMLS AlSi10Mg Aluminum · Thermal expansion: mean 25-100 °C, ASTM E228
- 2INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
- 3RenAM 500 Series Aluminium AlSi10Mg Material Data SheetRenishawDMLS AlSi10Mg Aluminum · Young's modulus (stiffness): same material and process, different machine maker: Renishaw RenAM 500, 30 µm, as built, horizontal (XY)
- 4EOS Aluminium AlSi10Mg Material Data Sheet, FlexLine, M 290 (2018)EOS GmbHarchived copyDMLS AlSi10Mg Aluminum · Density: typical part density (ISO 3369), EOS M 290, AlSi10Mg_030_FlexM291 (30 µm)
- 5MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseDMLS AlSi10Mg Aluminum · Poisson's ratio: base material: cast Al-Si-Mg alloy 359.0 (Al-9Si-0.6Mg, closest MIL-HDBK-5J alloy to AlSi10Mg / EN AC-43000)DMLS AlSi10Mg Aluminum · Specific heat: base material: cast Al-Si-Mg alloy 359.0 (MIL-HDBK-5J), at 100 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
DMLS AlSi10Mg Aluminum is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is DMLS AlSi10Mg Aluminum stronger than Nickel Inconel 718?
Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 270 MPa for DMLS AlSi10Mg Aluminum (4.47x).
Which is lighter, DMLS AlSi10Mg Aluminum or Nickel Inconel 718?
DMLS AlSi10Mg Aluminum is lighter: 2,670 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, DMLS AlSi10Mg Aluminum or Nickel Inconel 718?
Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 72 GPa for DMLS AlSi10Mg Aluminum, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, DMLS AlSi10Mg Aluminum or Nickel Inconel 718?
For the same stiffness or strength: DMLS AlSi10Mg Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong beam, strong panel or plate; Nickel Inconel 718 is lighter for a strong rod or tie.
| Part that must be | DMLS AlSi10Mg Aluminum | Nickel Inconel 718 |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 11% heavier |
| Stiff beam (bending) | lighter | 1.85x heavier |
| Stiff panel or plate | lighter | 2.19x heavier |
| Strong rod or tie | 45% heavier | lighter |
| Strong beam | lighter | 13% heavier |
| Strong panel or plate | lighter | 46% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, DMLS AlSi10Mg Aluminum or Nickel Inconel 718?
Nickel Inconel 718 stretches further before it breaks: 20% elongation at break against 10.2% for DMLS AlSi10Mg Aluminum.
Thermal
Which conducts heat better, DMLS AlSi10Mg Aluminum or Nickel Inconel 718?
DMLS AlSi10Mg Aluminum conducts heat better: 110 W/m·K against 11.4 W/m·K for Nickel Inconel 718.
Which expands less with temperature?
Nickel Inconel 718 expands less: 13.2 µm/m·K against 20 µm/m·K for DMLS AlSi10Mg Aluminum.
Related comparisons
- DMLS AlSi10Mg Aluminum vs. Aluminum
- DMLS AlSi10Mg Aluminum vs. Aluminum 6061-T6
- DMLS AlSi10Mg Aluminum vs. Aluminum 2024-T351
- DMLS AlSi10Mg Aluminum vs. Aluminum 6063-T6
- Nickel Inconel 718 vs. Stainless Steel 17-4PH
- Nickel Inconel 718 vs. Steel AISI 4340
- Nickel Inconel 718 vs. DMLS 17-4PH Stainless Steel
- Nickel Inconel 718 vs. Steel AISI 1045