Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
Plastic PEEK
Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)
1
INCONEL alloy 718 (SMC-045)Special Metalsarchived copyNickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer
2
VICTREX PEEK 450G Technical Data SheetVictrexPlastic PEEK · Yield strength: typical, tensile yieldPlastic PEEK · Compressive strength: typical, 23 CPlastic PEEK · Flexural strength: typical, flexural stress at yield, 23 CPlastic PEEK · Elongation at break: typical, at breakPlastic PEEK · Young's modulus (stiffness): typical (nominal)Plastic PEEK · Density: typical (crystalline)Plastic PEEK · Thermal conductivity: typical, average, 23 CPlastic PEEK · Thermal expansion: average of flow/cross-flow, below Tg (<143 C)Plastic PEEK · Melting point: typical, DSCPlastic PEEK · Glass transition: onset (midpoint 150 C)Plastic PEEK · Max service temperature: UL 746B RTI, mechanical strength (continuous use index)
3
VICTREX PEEK for Use in Fluid Management (2020)VictrexPlastic PEEK · Poisson's ratio: typical
4
VICTREX PEEK 450G Technical Data Sheet (2012)Victrexarchived copyPlastic PEEK · Specific heat: typical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Nickel Inconel 718 stronger than Plastic PEEK?
Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 98 MPa for Plastic PEEK (12.3x).
Which is lighter, Nickel Inconel 718 or Plastic PEEK?
Plastic PEEK is lighter: 1,300 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Plastic PEEK?
Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 4 GPa for Plastic PEEK, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Plastic PEEK?
For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie; Plastic PEEK is lighter for a stiff panel or plate, strong beam, strong panel or plate.
Part that must be
Nickel Inconel 718
Plastic PEEK
Stiff rod or tie (tension)
lighter
7.91x heavier
Stiff beam (bending)
lighter
12% heavier
Stiff panel or plate
1.72x heavier
lighter
Strong rod or tie
lighter
1.95x heavier
Strong beam
19% heavier
lighter
Strong panel or plate
1.8x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Nickel Inconel 718 or Plastic PEEK?
Plastic PEEK stretches further before it breaks: 25% elongation at break against 20% for Nickel Inconel 718.
Thermal
Which conducts heat better, Nickel Inconel 718 or Plastic PEEK?
Nickel Inconel 718 conducts heat better: 11.4 W/m·K against 0.29 W/m·K for Plastic PEEK.
Which expands less with temperature?
Nickel Inconel 718 expands less: 13.2 µm/m·K against 55 µm/m·K for Plastic PEEK.