Materials / Compare
Nickel Inconel 718 vs. Plastic PETG Compare Nickel Inconel 718 vs. Plastic PETG strength, stiffness, weight and thermal properties.
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Nickel Inconel 718 Wrought Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Plastic PETG 3D printed (FDM) Mechanical Nickel Inconel 718 Plastic PETG Yield strength 1,207 MPa 26.1x stronger 46.2 MPa Ultimate tensile strength 1,389 MPa 30.1x stronger 46.2 MPa Flexural strength not sourced 78.9 MPa Elongation at break 20 % 2.63x more ductile 7.6 % Young's modulus (stiffness) 200 GPa 103x stiffer 1.94 GPa Density 8,221 kg/m³ 1,270 kg/m³ 6.47x lighter Strength to weight 147 kN·m/kg 4.04x higher 36.4 kN·m/kg Stiffness to weight 24.3 MN·m/kg 15.9x higher 1.53 MN·m/kg Poisson's ratio 0.294 not sourced Shear modulus 77.3 GPa not sourced Bulk modulus 162 GPa not sourced Speed of sound 4,932 m/s 3.99x faster 1,236 m/s
1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic ABS Plastic TPU Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic PETG Stiffness against densityHigher and further left: stiffer for its weight 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic ABS Plastic TPU Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic PETG Strength against densityHigher and further left: stronger for its weight
Thermal Nickel Inconel 718 Plastic PETG Thermal conductivity 11.4 W/m·K 54.3x more heat through a fin base material 0.21 W/m·K Thermal expansion 13.2 µm/m·K 3.86x less base material 51 µm/m·K 100 mm part over a 50 °C swing 66 µm growth 3.86x less 255 µm growth Specific heat 435 J/kg·K base material 1,300 J/kg·K 2.99x higher Heats up and cools (diffusivity) 3.19 mm²/s 25.1x faster 0.127 mm²/s Thermal shock resistance 3,680 W/m not sourced Melting point melting range 1,260–1,336 °C not sourced Glass transition not sourced 77.4 °C Max service temperature 704 °C HDT 0.455 MPa 76.2 °C
1k 10k 0.1 1 10 100 Density (kg/m³) Thermal conductivity (W/m·K) Plastic PLA Plastic ABS Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic PETG Thermal conductivity against densityHigher and further left: spreads more heat for its weight 0.1 1 10 100 10 100 Thermal conductivity (W/m·K) Thermal expansion (µm/m·K) Plastic ABS Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Nickel Inconel 718 Plastic PETG Thermal expansion against thermal conductivityLower and further right: warps less when heated
Sources 3 documents: Special Metals, UltiMaker, Eastman
Nickel Inconel 718 INCONEL alloy 718, standard grade, 1750 °F/1 hr anneal + 1325 °F/8 hr F.C. to 1150 °F aged; Special Metals bulletin SMC-045 typical values
Plastic PETG Ultimaker PETG, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v1.00, April 29, 2022. 1 INCONEL alloy 718 (SMC-045) Special Metals archived copy Nickel Inconel 718 · Yield strength: typical, 1.0 in. hot-rolled bar, 0.2% offsetNickel Inconel 718 · Ultimate tensile strength: typical, 1.0 in. barNickel Inconel 718 · Elongation at break: typical, 1.0 in. barNickel Inconel 718 · Young's modulus (stiffness): typical, 21 °C, annealed + agedNickel Inconel 718 · Density: nominal, annealed and agedNickel Inconel 718 · Poisson's ratio: typical, 21 °C, annealed + agedNickel Inconel 718 · Thermal conductivity: typical, 21 °C, annealed + aged (calculated from resistivity per footnote a)Nickel Inconel 718 · Thermal expansion: typical, mean 21-93 °C, annealed + agedNickel Inconel 718 · Specific heat: typical, 21 °CNickel Inconel 718 · Melting point: melting rangeNickel Inconel 718 · Max service temperature: upper use temperature stated by producer2 Ultimaker PETG Technical Data Sheet, v1.00 UltiMaker archived copy Plastic PETG · Yield strength: typicalPlastic PETG · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic PETG · Flexural strength: typicalPlastic PETG · Elongation at break: typicalPlastic PETG · Young's modulus (stiffness): typicalPlastic PETG · Density: typicalPlastic PETG · Glass transition: typicalPlastic PETG · Max service temperature: HDT 0.455 MPa (printed specimens)3 Eastar Copolyester 6763 Product Data Sheet Eastman Plastic PETG · Thermal conductivity: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Thermal expansion: base material: Eastman Eastar Copolyester 6763 (PETG), typicalPlastic PETG · Specific heat: base material: Eastman Eastar Copolyester 6763 (PETG), DSC at 60 °C (lowest temperature listed)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Plastic PETG is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions Mechanical Is Nickel Inconel 718 stronger than Plastic PETG? Nickel Inconel 718 is stronger: its yield strength is 1,207 MPa against 46.2 MPa for Plastic PETG (26.1x).
Which is lighter, Nickel Inconel 718 or Plastic PETG? Plastic PETG is lighter: 1,270 kg/m³ against 8,221 kg/m³ for Nickel Inconel 718.
Which is stiffer, Nickel Inconel 718 or Plastic PETG? Nickel Inconel 718 is stiffer: Young's modulus 200 GPa against 1.94 GPa for Plastic PETG, so the same part in Nickel Inconel 718 deflects less under the same load.
Which is lighter for the same job, Nickel Inconel 718 or Plastic PETG? For the same stiffness or strength: Nickel Inconel 718 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam; Plastic PETG is lighter for a stiff panel or plate, strong panel or plate.
Part that must be Nickel Inconel 718 Plastic PETG Stiff rod or tie (tension) lighter 15.9x heavier Stiff beam (bending) lighter 1.57x heavier Stiff panel or plate 38% heavier lighter Strong rod or tie lighter 4.04x heavier Strong beam lighter 36% heavier Strong panel or plate 27% heavier lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Nickel Inconel 718 or Plastic PETG? Nickel Inconel 718 stretches further before it breaks: 20% elongation at break against 7.6% for Plastic PETG.
Thermal Which conducts heat better, Nickel Inconel 718 or Plastic PETG? Nickel Inconel 718 conducts heat better: 11.4 W/m·K against 0.21 W/m·K for Plastic PETG.
Which expands less with temperature? Nickel Inconel 718 expands less: 13.2 µm/m·K against 51 µm/m·K for Plastic PETG.